Reliability evaluation of Pb-free solder joints combining Sn-Bi-Ag and Sn-Ag-Cu solders
- Journal
- Journal of Materials Science: Materials in Electronics impact factor
- Status
- Published
- Vol
- 37
- Page
- 2227
- Year
- 2026
- Link
- https://doi.org/10.1007/s10854-026-18659-x 98회 연결
Pb-free solder joints combining Sn-3.0Ag-0.5Cu (SAC305) solder balls with low-melting-temperature Sn-57Bi-1Ag solder paste offer a potential approach to reducing reflow temperature while maintaining joint reliability. However, the effects of reflow temperature on Bi redistribution, interfacial reactions, and mechanical reliability remain insufficiently understood. In this study, SAC305/Sn-57Bi-1Ag solder joints were fabricated using three reflow profiles with peak temperatures of approximately 190, 210, and 260 °C. Joint microstructures and elemental distributions were characterized by scanning electron microscopy, energy-dispersive X-ray spectroscopy, and electron probe microanalysis. Reliability was evaluated by thermal shock testing from − 40 to 85 °C for up to 2,000 cycles, followed by low-speed shear testing and fracture analysis. Bi diffusion was limited in the as-reflowed Type 1 and Type 2 joints became more pronounced toward the package side with increasing thermal shock cycles, whereas Bi was uniformly distributed in the Type 3 joints because of the higher reflow temperature. Cu6Sn5 and (Cu, Ni)6Sn5 intermetallic compounds formed at the package and PCB interfaces, respectively, and their thicknesses changed with thermal shock cycling. The shear strength of the Type 1 and Type 3 joints decreased during thermal shock testing, whereas that of the Type 2 joints gradually increased. Fracture analysis further revealed reflow-condition-dependent changes in fracture location. These results demonstrate that reflow temperature strongly influences Bi redistribution, interfacial evolution, and the mechanical reliability of SAC305/Sn-57Bi-1Ag solder joints.